Views: 0 Author: Site Editor Publish Time: 2026-11-27 Origin: Site
4. Three Technical Approaches
Esko, Kodak (Miraclon), and XSYS have achieved highly consistent physical Microcell structures through three entirely different engineering approaches. Understanding these differences is essential to understanding why their requirements for flexographic plate materials vary so significantly.
4.1 ESKO: The “In-Situ Generation” Approach Through Laser Energy Modulation
Technical Architecture
- ESKO Microcells are generated directly on the CDI laser imager, an approach known as “in-situ generation.” The RIP (Imaging Engine) encodes the Microcell patterns into 1-bit TIFF, LEN, or LENX files. The CDI then ablates the LAMS black mask according to the pattern, followed by UV main exposure and plate washing, forming microcavities in the polymer surface.
- The key challenge is that each Microcell consists of only 1–4 pixels. At 4000 ppi, one pixel measures approximately 6.35 μm. The nominal laser energy density (approximately 3.2 J/cm²) is insufficient to completely open the black mask layer in such a small area.
- ESKO addresses this issue through Pixelboost energy enhancement. Additional energy is applied to single-pixel Microcells, with the boost level exposed as an adjustable parameter on the CDI. The Boost Editor provides three dedicated settings: Microscreen, Groovy, and Quartz Pixel+.
- Engineering Significance of Pixelboost
For the same Microcell pattern, the optimal boost energy changes with the plate material, CDI unit, and plate-washing conditions. This is not a parameter that can be “set once and used indefinitely.” Instead, energy levels must be validated against established standards and verification intervals.ESKO specifies three evaluation criteria:1. No trailing-edge voids.2. A smooth, uniform ink film without clouding or pinholes.3. Maximum solid ink density (SID).
Pattern Code | Structure Type | Applications | Description |
MCWSI | Inverse Microcells | General Solids / Shadows | Classic Microscreen pattern series featuring single-pixel microcell arrays; the primary default pattern for Pixel+. |
MG34/MG25/MG45 | Grooves (Groovy) | Large Solid Areas / High Ink Volumes | Linear ink-transfer structure with higher ink-carrying capacity than inverse Microcells; has an independent boost parameter on the CDI (Groovy). |
WSI | Inverse Microcells | Solids + Text and Linework | Dedicated pattern introduced with the new 1400 lpi laser technology, offering cleaner edge handling. |
Q-Cells(classic) | Inverse Microcells | General-Purpose Crystal / Quartz | The primary pattern of the 2000 lpi era; requires the CDI Crystal Quartz Edition (Q-Optics). |
vQ/sQ | Inverse Microcells | Highlights / Stochastic Screening | VQ = Variable Highlight Q-Cells; SQ = Stochastic Q-Cells, introduced with the Quartz Edition. |
MC16P | Inverse Microcells | UV White Ink | PCW’s dedicated UV white-ink pattern (not the Crystal white-ink pattern chart for Quartz). |
Table 4-1 ESKO Microcell Pattern Families. White ink uses a dedicated pattern system—the PCW white-ink test chart includes A (reference without Microcells) plus eight Microcell patterns, B–I.
4.2 Kodak / Miraclon: The “Pattern Transfer” Approach Using a Laminated Mask
Technical Architecture
- Flexcel NX does not image the plate material directly. Instead, it images a thermal imaging layer (TIL). A SquareSpot laser writes the pattern onto the film, which is then laminated onto the printing plate. The lamination process performs two functions simultaneously: transferring the pattern and excluding oxygen. Once oxygen inhibition is eliminated, UV exposure produces true 1:1 flat-top dots, theoretically eliminating the need for bump curves to “guess” the minimum printable dot.
- Miraclon’s method is compatible only with its own plate materials and cannot be used with plates from other manufacturers. Its Microcell screening system is a closed-loop system that relies on its own laser imager, plate processor, plate materials, and other components.
- DigiCap NX Patterning is a software-based feature. It superimposes an ultra-fine structured texture across the surface of all image elements on the plate. The pattern elements measure approximately 5 × 10 μm and are produced using the exceptionally high optical engraving resolution of SquareSpot technology.
Version / Feature | Period | Function |
FLEXCEL NX System | 2008 | TIL lamination and oxygen exclusion achieve 1:1 flat-top dots, introducing the industry’s first digital flat-top dot solution. |
DigiCap NX | 2009-2010 | The first commercialized surface patterning technology, using a 5 × 10 μm texture across all image elements. |
NX Advantage Advanced DigiCap | 2015-2016 | Introduces Advanced Edge Definition, optimizing ink flow according to image-element type to improve contrast. |
FLEXCEL NX UItra | 2018 | Aqueous-processing version that brings flat-top dots and surface patterning to solvent-free plate making. |
PureFlexo Printing | 2021 | Shifts the focus from “increasing ink transfer” to “suppressing unwanted ink spread,” controlling dot bridging, trailing-edge defects, and ink starvation. |
Table 4-2 Evolution of Kodak/Miraclon Surface Patterning Technology. In 2021, the FLEXCEL NX business was spun off from Kodak to form Miraclon, while the product branding continued to use KODAK FLEXCEL NX.
Key Characteristics of This Approach:
- Advantages: Exceptional 1:1 flat-top dot quality, stable minimum dots, and theoretically no need for bump curves; high patterning precision; the same plate material can cover applications ranging from corrugated packaging to flexible packaging.
- Limitations: A closed system—requires Flexcel NX plates, a SquareSpot imager, and TIL film, with no compatibility for reuse on third-party equipment; adds a lamination step and consumable costs.
4.3 XSYS: The “Open-System” Approach to Surface Screening at the Imager
Technical Architecture
- The ThermoFlexX Woodpecker directly superimposes high-frequency surface microstructures (SuS) onto the plate image during the imaging stage, with a typical optical resolution of 5080 dpi. Its positioning is clear: it is not tied to a specific RIP or workflow and accepts TIFF or LEN files directly, allowing it to integrate into virtually any existing prepress workflow.
- An important design trade-off is that the pattern is not embedded in the file but superimposed during imaging, effectively applying a second screening stage after the RIP. This avoids excessive file sizes caused by ultra-high-frequency patterns and significantly reduces data-processing time—a key engineering detail that makes the “open-system” approach practical.
Variant | Input Resolution | Flat-Top Requirements | Positioning |
Sharp | 2400 / 2540 dpi | Compatible with either tube or LED main exposure | All-round solution. Screening frequency matches well with anilox rollers and supports four-color process, extended color gamut (ECG), and spot-color halftones. SID improvement is comparable to Nano. Easiest to implement. |
Nano | 2000 dpi | Requires high-power LED exposure (Catena-E) or nyloflex FTV with a lamp output of >20 mW | Finest pattern available for LAMS plates. Suitable for plate rooms seeking the highest possible screening frequency. Offers better symmetry and a lower probability of interference with halftone dots. |
Nevis | - | Same flat-top requirements | Dedicated white-ink solution featuring three coarseness levels and automatically generated test charts for pattern selection. Designed to improve white-ink opacity, eliminate pinholes, and reduce ink consumption. |
Replay | 4000 dpi | Same flat-top requirements | For users with established SuS workflows. Automatically detects single-pixel patterns in files and applies an energy boost to reproduce them accurately on ThermoFlexX imagers. |
Table 4-3 Four Woodpecker Variants. Key Engineering Principle: High-frequency SuS should be paired with high-line-count, low-volume anilox rollers; low-frequency SuS should be paired with low-line-count, high-volume anilox rollers, especially for white ink.
Interference Risk (Explicitly Highlighted in XSYS Official Documentation)
Surface screening is superimposed on halftone dots, so interference between the two is inevitable, potentially manifesting as moiré patterns. XSYS provides a list of validated line-screen and angle combinations. Some older TIFF/LEN files may not be compatible.
In addition, when halftones are combined with SuS using Catena-E exposure, only a very small bump-up is required (typically less than 1% at 150 lpi). Tube exposure requires a higher bump-up, depending on the plate material and light intensity.